| Title | Bakelite Sample Disc |
| Object Name | Bakelite Sample Disc |
| Manufactured By | Bakelite Corp.
|
| Description | Degraded cellulose acetate made in CA pilot plant 1938- 1941. Degradation probably cause by insufficient washing of acid over 70 plus years. A residue of H2SO4 (Sulfuric acid) catalyst has caused the obvious damage. It is not generally known that Bakelite attempted to get into this thermoplastic field. |
| Date Manufactured | 1938- 1941 |
| Material | Cellulose Acetate |
| Manufacturing Process | Compression Molded, Compression Press, Hydraulic. Control Hydraulic Pressure System. |
| Number of Objects | 1 |
| Accession Number | 2011.066.01 |
| Donor | Gift of George Marshall Naul |
| Broad Subject | Material Samples
|
| Subjects | Plastic Manufacturing
|
| For More Information | Please address inquires to the Public Services Librarian, Special Collections Research Center, Syracuse University Library (e-mail: scrc@syr.edu, tel. 315-443-2697). |
| Rights | Publication of images from the Special Collections Research Center is subject to approval and fees may be charged for such use. Publication includes the following media: print, electronic/digital, videotape, film, or microfilm. Permission to use images must be obtained in advance and in writing from the Special Collections Research Center by writing to plastics@syr.edu or going to http://scrc.syr.edu . These fees are separate from any which might be assigned/assessed by the copyright holder. |
|
|
|
|
|